Nanoscale, 2015, Advance Article
DOI: 10.1039/C5NR06264K, Paper
C.-Y. Su, C.-C. Wang, Y.-C. Hsueh, V. Gurylev, C.-C. Kei, T.-P. Perng
Parallel arrays of Zn-doped TiO2 nanotubes fabricated via nanolaminated packing of alternating layers of TiO2 and ZnO by ALD using polycarbonate as a template are presented. A uniform bulk solubility of [similar]8 at% was achieved, far beyond the nil solubility predicted by the phase diagram.