Nanoscale, 2015, Advance Article
DOI: 10.1039/C5NR05392G, Paper
Kyung Sun Park, Sejoon Kim, Hongbum Kim, Deokhyeon Kwon, Yong-Eun Koo Lee, Sung-Wook Min, Seongil Im, Hyoung Joon Choi, Seulky Lim, Hyunjung Shin, Sang Man Koo, Myung Mo Sung
ZnO-stitched CVD graphene with well-connected grains shows excellent mobility with remarkable device-to-device uniformity on a large-area substrate.